On Oct 15, 9:35pm, "Jeremy Pinwhistle" <pinwhis
...@micorsoft.com> wrote:
> Hi,
> Could someone advise me on what type of tools/kit I need to buy for shaping
> small pieces of stone please?
> The material is really soft - it can be scratched with a point of a nail,
> and can be cut with an ordinary hacksaw/ drill.
> What I would like is to make small (around 1cm to 3cm) figurines from it, so
> that they can hang as necklaces. I would need to sculpt them and obviously
> drill then for a chain. Maybe even a small brooch. This is only for
> Christmas pressies - not a commercial venture - however I would like good
> quality equipment. Also some sort of vice/magnifier to hold/see the pieces
> to work on - presumably some type of jaws that would not mark the stone.
> I do have ordinary air tools/compressor in the workshop, and wondered if
> there were any small tools that could be connected to the airline?
> Thanks for reading this and for any advice you can offer.
> Regards,
> Steve.
What part of Texas are you in. There is a gem and mineral club with
all kinds of tools for cutting stone in Arlington TX. After becoming a
member the cost for using the tools is around $10 an hour.
Additionally, there is a gem club in Garland Tx. Any type of diamond
bit burs will work, while using water to keep the stone wet. If the
stone or bur gets too hot, the bur will dull or the stone breaks.
Harbor Freight has a very cheep set of different shape diamond burs.
They don't last too long on hard stones (you get what you pay for).
But, if as you say the stone cuts easily, then these should do you
fine. For polishing the stone, if its not too soft you can use a small
cotton buff and Zam to polish. You can buy Zam at any jewelry supply.
Rio Grande sells some at
www.riogrande.com. Here are some stock
numbers. The Zam is a polish that you put on a buff while it is
spinning, # 331-123 Cost $6.20. Diamond bur set # 346-064 $14.95,
Miniature buff set # 330-614 Cost $ 9.80. Hope that helps.
Janet Alexander
Check out my on-line free tutorials at by blogg The Jewelery
Classroom: http://thejewelryclassroom.ning.com/