I'm helping a partially blind friend. He has some small pieces of polished Brazilian quartz he wants to drill a hole into. I have found several suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable prices, around $15 per. Slightly less when bought in threes.
Is this what he needs to drill these holes? I know he needs to use coolant, and set it up in a drill press. Info on what would be the best way to do this appreciated.
On Sat, 12 Sep 2009 01:06:47 -0700, in rec.crafts.jewelry "SteveB"
<oldf...@depends.com> wrote: >>I'm helping a partially blind friend. He has some small pieces of polished >>Brazilian quartz he wants to drill a hole into. I have found several >>suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable >>prices, around $15 per. Slightly less when bought in threes.
>>Is this what he needs to drill these holes?
Possibly. He/you do need diamond drills, but beware of the chinese made ones which are an ordinary twist drill coated with diamonds. Those won't do the job. What you need are either "wire" drills (small sizes) or "core" drills, which are tubes coated on the front edge with diamond. The wire bits are steel wire similarly coated at the end with diamond. Better ones are not coated, but tipped with a piece of sintered meta/diamond mix, which means the diamonds go into the metal a bit, rather than being just a surface electroplated coating. Make sure that the drills you get are intended for lapidary use, or drilling glass (similar, though easier).
>> I know he needs to use coolant,
Generally, water is fine. If you're doing a lot of this, you'd add a corrosion inhibitor to the water. One way to do this is to use lapidary dop wax (like sealing wax), or a glue, to affix the stones to the bottom of a glass ashtray, or some similar vessel you can afford to damage. The stone then can be covered in water, so the drilling takes place submerged. And being affixed to the glass container helps prevent chipping when the drill breaks through the back side.
>>and set it up in a drill press. Info on what would be the best way to do >>this appreciated.
High speed, but little pressure. You bring the drill down to work for a few seconds, then briefly lift it up a tad, to allow coolant to flush out drillings and keep the bottom of the hole cool, then come down again. Repeat till done.
Both Crystalite and Lapcraft corporations make good quality lapidary diamond drills, and there are no doubt others too. Like I said, try to avoid the really cheap chinese stuff. They just don't last so long on stone.
> On Sat, 12 Sep 2009 01:06:47 -0700, in rec.crafts.jewelry "SteveB" > <oldf...@depends.com> wrote:
>>>>I'm helping a partially blind friend. He has some small pieces of polished >>>>Brazilian quartz he wants to drill a hole into. I have found several >>>>suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable >>>>prices, around $15 per. Slightly less when bought in threes.
>>>>Is this what he needs to drill these holes?
>>Possibly. He/you do need diamond drills, but beware of the chinese made ones >>which are an ordinary twist drill coated with diamonds. Those won't do the job. >>What you need are either "wire" drills (small sizes) or "core" drills, which are >>tubes coated on the front edge with diamond. The wire bits are steel wire >>similarly coated at the end with diamond. Better ones are not coated, but >>tipped with a piece of sintered meta/diamond mix, which means the diamonds go >>into the metal a bit, rather than being just a surface electroplated coating. >>Make sure that the drills you get are intended for lapidary use, or drilling >>glass (similar, though easier).
>>>> I know he needs to use coolant,
>>Generally, water is fine. If you're doing a lot of this, you'd add a corrosion >>inhibitor to the water. One way to do this is to use lapidary dop wax (like >>sealing wax), or a glue, to affix the stones to the bottom of a glass ashtray, >>or some similar vessel you can afford to damage. The stone then can be covered >>in water, so the drilling takes place submerged. And being affixed to the glass >>container helps prevent chipping when the drill breaks through the back side.
>>>>and set it up in a drill press. Info on what would be the best way to do >>>>this appreciated.
>>High speed, but little pressure. You bring the drill down to work for a few >>seconds, then briefly lift it up a tad, to allow coolant to flush out drillings >>and keep the bottom of the hole cool, then come down again. Repeat till done.
>>Both Crystalite and Lapcraft corporations make good quality lapidary diamond >>drills, and there are no doubt others too. Like I said, try to avoid the really >>cheap chinese stuff. They just don't last so long on stone.
>>Peter
>>>Steve
We went to the glass shop yesterday to get some glass cut. Fred asked the man, and he brought out a bit that cut a 1/8" hole. It looked like a core drill, just miniature. Straight shoulders on the end of the bit. He cut the hole with a hand drill. So, I believe what I am looking for is straight sided core drill bits, just smaller ones. I am now researching prices, and will look at the places you mentioned. We are going to cut holes in thin slabs of Brazilian agate to make wind chimes.
>>We went to the glass shop yesterday to get some glass cut. Fred asked the >>man, and he brought out a bit that cut a 1/8" hole. It looked like a core >>drill, just miniature. Straight shoulders on the end of the bit. He cut >>the hole with a hand drill. So, I believe what I am looking for is straight >>sided core drill bits, just smaller ones. I am now researching prices, and >>will look at the places you mentioned. We are going to cut holes in thin >>slabs of Brazilian agate to make wind chimes.
>>Steve
Glass is softer than agate, and easier to drill, but the equipment is similar. A hand drill will be quite tedius with agate, even if practical for glass, but it would work if you don't have many holes to drill. Whether you will be using a core bit (a tube) or a solid wire bit depends on the size of the hole you need. Core bits are only made down to a certain size, and only offer an advantage in sizes where leaving the center core intact instead of grinding it away, saves a significant amount of grinding. The professional glass drilling rigs use a drill press that can force water down through the core tube while drilling, thus improving lubrication and removal of the grindings, but that's normally overkill and not used for small holes such as you'd need to hang slabs of agate from a wind chime design.
Also, Lapcraft and Crystalite are manufacturers, not places. they're generally wholesale sellers, so what you'll likely find are resellers who carry those brands.... They're primarily manufacturers of lapidary (stone cutting) diamond tools of a number of sorts. Companies who's web sites you might check that occur to me off hand, would be Kingsley North, Rio Grande, Gesswein, or others who carry not just jewelry making, but lapidary supplies.
> On Sat, 12 Sep 2009 12:49:06 -0700, in rec.crafts.jewelry "SteveB" > <oldf...@depends.com> wrote:
>>Also, Lapcraft and Crystalite are manufacturers, not places. they're generally >>wholesale sellers, so what you'll likely find are resellers who carry those >>brands.... They're primarily manufacturers of lapidary (stone cutting) diamond >>tools of a number of sorts. Companies who's web sites you might check that >>occur to me off hand, would be Kingsley North, Rio Grande, Gesswein, or others >>who carry not just jewelry making, but lapidary supplies.
Thanks for the help. This is a simple deal, but as we live in a small rural town, it will be much easier to mail order than go to town. Crystalite doesn't even list a distributor in Utah.
Steve
The only sorts of retailers who'd carry this sort of thing would be jewelry or lapidary supply shops. There aren't that many anyway, who are still "brick and morter" shops in most cities. The internet is the place to look in any case, which is what I was intending with those references.
Interesting cheap, small core drill set from Rio. Don't know quality. They also sell lots of the twist drills which I don't like so much for stone (fine for glass and ceramic, but I find they dull too quickly with tough materials like stone) http://www.riogrande.com/MemberArea/ProductPage.aspx?assetname=349016...1252796012042=diamond+drills (be sure you use the entire URL, including the bit after the word "text". My mail program seems to want to break it there...)
SteveB wrote: > I'm helping a partially blind friend. He has some small pieces of polished > Brazilian quartz he wants to drill a hole into. I have found several > suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable > prices, around $15 per. Slightly less when bought in threes.
> Is this what he needs to drill these holes? I know he needs to use coolant, > and set it up in a drill press. Info on what would be the best way to do > this appreciated.
> Steve
Now you have mentioned what the holes are for, ie hanging up the agate to make wind chimes, Have you considered any other way of hanging said agate? There are many other solutions to this question, I list a few that come to mind 1. use some wire to make a "U" shaped loop with the wire ends bent back on themselves to increase the contact area on the agate sides. Then 2 part epoxy to the agate. 2. a similar idea but using some thin strip some 1/8 in wide by say 1/32 thick. Epoxy in place as in 1. 3. if the agate is say 1/2in wide by 1/8in thick, cut a groove each side into the 1/8in edge. String up using the grooves to hold the agate. Use the stone slitting saw to do this. 4. If you can do 3. above extend this idea to make a clip with rt/angle ends indexing in the slots. epoxy in place.
My local glass works use arrow end tungsten carbide to drill holes. Ive a set of diamond core drills the smallest is 1/6in od. Water is pumped down the core via a oring sealed head. Otherwise it goes into an ordinary drill press.
SteveB wrote: > I'm helping a partially blind friend. He has some small pieces of polished > Brazilian quartz he wants to drill a hole into. I have found several > suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable > prices, around $15 per. Slightly less when bought in threes.
> Is this what he needs to drill these holes? I know he needs to use coolant, > and set it up in a drill press. Info on what would be the best way to do > this appreciated.
> Steve
Now you have mentioned what the holes are for, ie hanging up the agate to make wind chimes, Have you considered any other way of hanging said agate? There are many other solutions to this question, I list a few that come to mind 1. use some wire to make a "U" shaped loop with the wire ends bent back on themselves to increase the contact area on the agate sides. Then 2 part epoxy to the agate. 2. a similar idea but using some thin strip some 1/8 in wide by say 1/32 thick. Epoxy in place as in 1. 3. if the agate is say 1/2in wide by 1/8in thick, cut a groove each side into the 1/8in edge. String up using the grooves to hold the agate. Use the stone slitting saw to do this. 4. If you can do 3. above extend this idea to make a clip with rt/angle ends indexing in the slots. epoxy in place.
My local glass works use arrow end tungsten carbide to drill holes. Ive a set of diamond core drills the smallest is 1/6in od. Water is pumped down the core via a oring sealed head. Otherwise it goes into an ordinary drill press.
>>SteveB wrote: >>> I'm helping a partially blind friend. He has some small pieces of polished >>> Brazilian quartz he wants to drill a hole into. I have found several >>> suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable >>> prices, around $15 per. Slightly less when bought in threes.
>>> Is this what he needs to drill these holes? I know he needs to use coolant, >>> and set it up in a drill press. Info on what would be the best way to do >>> this appreciated.
>>> Steve
>>Now you have mentioned what the holes are for, ie hanging up the agate >>to make wind chimes, >>Have you considered any other way of hanging said agate? >>There are many other solutions to this question, >>I list a few that come to mind >>1. use some wire to make a "U" shaped loop with the wire ends bent back >>on themselves to increase the contact area on the agate sides. >> Then 2 part epoxy to the agate. >>2. a similar idea but using some thin strip some 1/8 in wide by say 1/32 >>thick. Epoxy in place as in 1. >>3. if the agate is say 1/2in wide by 1/8in thick, cut a groove each side >>into the 1/8in edge. String up using the grooves to hold the agate. >>Use the stone slitting saw to do this. >>4. If you can do 3. above extend this idea to make a clip with rt/angle >>ends indexing in the slots. epoxy in place.
>>My local glass works use arrow end tungsten carbide to drill holes. >> Ive a set of diamond core drills the smallest is 1/6in od. Water is >>pumped down the core via a oring sealed head. Otherwise it goes into an >>ordinary drill press.
>>hope this helps. >> Ted >>Dorset >>UK.
We have made polished agate slab wind chimes in the past using 'leaf' - type bails (basically a thin strip/rod with a leaf shape at each end, fold into a 'U' shape to fit slab) and good epoxy (Hughes or similar) We strung them with fishing line to some hobby/craft brass rings. They have endured many seasons outdoors in Texas so far.
If you decide to drill, you may get better 'tone' by drilling the holes 2/9 of the way down from the top. measure the long axis (in millimeters) calculate 2/9 the distance and 'pinch' the slab there and strike it - probably get a better tone that pinching it anywhere else. They will work fine regardless - but try it and see what you think.
On Sep 12, 1:06am, "SteveB" <oldf...@depends.com> wrote:
> I'm helping a partially blind friend. He has some small pieces of polished > Brazilian quartz he wants to drill a hole into. I have found several > suppliers on line that will sell 1/16" and 1/8" diamond bits for reasonable > prices, around $15 per. Slightly less when bought in threes.
> Is this what he needs to drill these holes? I know he needs to use coolant, > and set it up in a drill press. Info on what would be the best way to do > this appreciated.
> Steve
Steve - if you want a source that is probably local - Lasco Diamond has reps across the country - if you happen to be in the SFV, CA area - you could even get a demo. They will be at the Woodland Hills RockChipper Show in Oct.
Lasco is the diamond bits used in Lapidary, the Nail Industry (as in Acrylic Finger Nails - not hammering nails) and in the Dental Industry...there website is: http://www.lascodiamond.com/